Flexural Modulus 2.97 - 2.97 GPa

@Temperature 120 - 120 °C
431 - 431 ksi

@Temperature 248 - 248 °F
Average value: 2.97 GPa Grade Count:1
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re..