Polymer Property : Flexural Modulus = 2.892 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.892 GPa
419.5 ksi
ASTM D790
A. Schulman POLYFLAM™ E-15937B High Strength Impact Modified Polypropylene
DescriptionPolyfort® E-15937B is a high strength impact modified polypropylene.Information provided by A. Schulman.
Flexural Modulus 2.892 GPa
419.5 ksi
ASTM D790
A. Schulman POLYFLAM™ E-15937B High Strength Impact Modified Polypropylene
DescriptionPolyfort® E-15937B is a high strength impact modified polypropylene.Information provided by A. Schulman.
Flexural Modulus 2.892 GPa
419.5 ksi
ASTM D790
A. Schulman POLYFLAM™ E-15937B High Strength Impact Modified Polypropylene
DescriptionPolyfort® E-15937B is a high strength impact modified polypropylene.Information provided by A. Schulman.
Flexural Modulus 2.892 GPa
419.5 ksi
ASTM D790
A. Schulman POLYFLAM™ E-15937B High Strength Impact Modified Polypropylene
DescriptionPolyfort® E-15937B is a high strength impact modified polypropylene.Information provided by A. Schulman.
Flexural Modulus 2.892 GPa
419.5 ksi
ASTM D790
A. Schulman POLYFLAM™ E-15937B High Strength Impact Modified Polypropylene
DescriptionPolyfort® E-15937B is a high strength impact modified polypropylene.Information provided by A. Schulman.
Flexural Modulus 2.892 GPa
419.5 ksi
ASTM D790
A. Schulman POLYFLAM™ E-15937B High Strength Impact Modified Polypropylene
DescriptionPolyfort® E-15937B is a high strength impact modified polypropylene.Information provided by A. Schulman.