Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.749 GPa @Thickness 3.17 mm |
398.7 ksi @Thickness 0.125 in |
chs 0.05 in/min; ASTM D790 |
Diamond Polymers DIAMALOY GLY 9020 Sheet Extrusion Grade Diamaloy GLY 9020 resin is a high-gloss, low impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, an.. |