Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.6487 GPa | 384.16 ksi | ASTM D790 |
E-Polymers TEKAPPO® JF2 Un-Reinforced Heat Resistant Chemical Resistance M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |