Flexural Modulus 2.617 GPa
379.6 ksi
ASTM D790
Kleerdex Kydex® P51 Acrylic/PVC Extrusion Compound  (discontinued **)
Profile extrusion compound for building productsApplications: Handrails, crashrails, bumper guards, corner guardsFeatures: Extruded profiles made with P51 are extremely resistant to harsh chemicals ..