Polymer Property : Flexural Modulus = 2.552 GPa
Polymer Property :
Flexural Modulus =
2.552 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
2.552
GPa
370.1
ksi
ASTM D790
NYCOA 436 PA 6
NSF rated general purpose molding gradeInformation provided by NYCOA, Inc.