Mechanical Properties Metric English Comments
Flexural Modulus 2.55 - 2.55037 GPa

@Temperature 149 - 150 °C
370 - 369.906 ksi

@Temperature 300 - 302 °F
Average value: 2.55 GPa Grade Count:2
Overview of materials for Thermoplastic Polyimide, Unfilled