Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.415 - 2.525 GPa | 350.3 - 366.2 ksi | ASTM D790M |
DSM Somos® NeXT Stereolithography (SLA) Prototyping Polymer Somos® NeXT combines stiffness and impact resistance which brings it close the performance of injection molded thermoplastics. It produces finished parts with tight tolerances and detailed features.. |