Mechanical Properties Metric English Comments
Flexural Modulus 0.0172 GPa
2.50 ksi
2% Secant, in accordance with ASTM D638; ASTM D790
M. Holland Company MAGMA® LM372-A LLDPE  (discontinued **)
Features: High Clarity, Good Flexibility, Good Flow, High Gloss, Good ToughnessProcessing Method: Injection MoldingInformation provided by M. Holland.