Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.384 GPa | 345.8 ksi | tangent; chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 3501 Black 1302 Injection Molding Grade Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |