Polymer Property : Flexural Modulus = 2.344 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.344 GPa
340.0 ksi
ASTM D790
Eastman Tenite Acetate 109E3V46022 Natural, Trsp Cellulose Acetate  (discontinued **)
Plasticizer 25%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.2% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..