Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.336 GPa | 338.8 ksi | tangent; chs 0.05 in/min; ASTM D790 |
Diamond Polymers ASA S124 ASA Weatherable Polymers Injection Molding Grade, Medium Modulus Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.336 GPa | 338.8 ksi | tangent; chs 0.05 in/min; ASTM D790 |
Diamond Polymers ASA S-210E ASA Weatherable Polymers Extrusion Molding Grade, Medium Modulus Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |