Polymer Property : Flexural Modulus = 2.2433 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.2433 GPa
325.37 ksi
ASTM D790
Network Polymers NPS 90-0304 Super High Impact Polystyrene
Description: Injection Molding GradeInformation provided by Network Polymers Inc.
Flexural Modulus 2.2433 GPa
325.37 ksi
ASTM D790
Network Polymers NPS 90-0304 F Super High Impact Polystyrene
Description: Injection Molding GradeInformation provided by Network Polymers Inc.