Polymer Property : Flexural Modulus = 2.167 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.01492 - 0.01494 GPa
2.164 - 2.167 ksi
FiberNide Nickel Aluminide Foam Atomic 22% Aluminum
Description: This Nickel aluminide foam has excellent high temperature strength, oxidation resistance, and conductivity. This unique combination of properties makes this foam particularly suitable f..