Flexural Modulus 2.098 GPa
304.3 ksi
ASTM D790
A. Schulman POLYFLAM™ E-15086-1B Mineral Impact Modified, Low Warp Polypropylene Black
DescriptionPolyfort® E-15086-1B is a mineral impact modified low warp polypropylene black.Information provided by A. Schulman.
Flexural Modulus 2.098 GPa
304.3 ksi
ASTM D790
A. Schulman POLYFLAM™ E-15086-1B Mineral Impact Modified, Low Warp Polypropylene Black
DescriptionPolyfort® E-15086-1B is a mineral impact modified low warp polypropylene black.Information provided by A. Schulman.
Flexural Modulus 2.098 GPa
304.3 ksi
ASTM D790
A. Schulman POLYFLAM™ E-15086-1B Mineral Impact Modified, Low Warp Polypropylene Black
DescriptionPolyfort® E-15086-1B is a mineral impact modified low warp polypropylene black.Information provided by A. Schulman.
Flexural Modulus 2.098 GPa
304.3 ksi
ASTM D790
A. Schulman POLYFLAM™ E-15086-1B Mineral Impact Modified, Low Warp Polypropylene Black
DescriptionPolyfort® E-15086-1B is a mineral impact modified low warp polypropylene black.Information provided by A. Schulman.
Flexural Modulus 2.098 GPa
304.3 ksi
ASTM D790
A. Schulman POLYFLAM™ E-15086-1B Mineral Impact Modified, Low Warp Polypropylene Black
DescriptionPolyfort® E-15086-1B is a mineral impact modified low warp polypropylene black.Information provided by A. Schulman.
Flexural Modulus 2.098 GPa
304.3 ksi
ASTM D790
A. Schulman POLYFLAM™ E-15086-1B Mineral Impact Modified, Low Warp Polypropylene Black
DescriptionPolyfort® E-15086-1B is a mineral impact modified low warp polypropylene black.Information provided by A. Schulman.