Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.372 GPa | 199.0 ksi | ASTM D790-95 |
Multibase Multi-Pro® 2510 XGW High Gloss Polypropylene PP High Gloss compound formulated for small appliances such as food-processors and coffee machines. This product is high heat stabilized for use in irons and other appliances with elevated temperat.. |