Polymer Property : Flexural Modulus = 19.38 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 19.38 GPa
2811 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP PF00C PA 6 (Asia Pacific)
LNP* Thermocomp* PF00C is a compound based on Nylon 6 resin containing Glass Fiber.
Flexural Modulus 19.38 GPa
2811 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP PF00C PA 6
LNP* THERMOCOMP* PF00C is a compound based on Nylon 6 resin containing 60% Glass Fiber.