Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.300 GPa | 188.5 ksi | 1% tangent, 0.05 in/min.; LAB033 |
ExxonMobil Mytex™ AS33L-07VS rubber modified polypropylene with good impact and flow properties for automotive exterior applications.Information provided by ExxonMobil Chemical |
|||
Flexural Modulus | 1.300 GPa | 188.5 ksi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0437C40L Calcium Reinforced |
|||
Flexural Modulus | 1.300 GPa | 188.5 ksi | ASTM D790 |
Aclo Accucomp Polypropylene HPO309L Homopolymer |
|||
Flexural Modulus | 1.300 GPa | 188.5 ksi | ASTM D790 |
Aclo Accuguard Polypropylene HP1369V2CSL Homopolymer Flame Retardant Copper Stabilized |
|||
Flexural Modulus | 1.300 GPa | 188.5 ksi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0436C30L1 Calcium Reinforced |