Polymer Property : Flexural Modulus = 18.82 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 18.82 GPa
2730 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP UCL36S PPA
LNP* LUBRICOMP* UCL36S is a compound based on Polyphthalamide resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Heat Stabilized, Electrically Con..
Flexural Modulus 18.82 GPa
2730 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP UCL36S PPA (Asia Pacific)
LNP* Lubricomp* UCL36S is a compound based on Polyphthalamide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Heat Stabilized, Electrically Cond..