Flexural Modulus 18.17 GPa
2635 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI
LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Modulus 18.17 GPa
2635 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI (Asia Pacific)
LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.