Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 18.1 GPa | 2630 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UFW49RS PPA (Europe-Africa-Middle East) LNP* Thermocomp* UFW49RS is a compound based on Polyphthalamide resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 18.1 GPa | 2630 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UFW49RSC PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UFW49RSC is a compound based on Polyphthalamide resin containing Glass Fiber, Mineral. Added features include: Heat Stabilized. |
|||
Flexural Modulus | 18.1 GPa | 2630 ksi | GB/T 9341-2008 |
Sichuan Deyang Haton® hMR61 Polyphenylene Sulfide, Glass & Mineral Reinforced Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Flexural Modulus | 18.1 GPa | 2630 ksi | ASTM D790 |
Unitika E-RUNG60 Ultra high-rigidity PA6, Dry Ultra high-rigidityInformation provided by Unitika Ltd. |
|||
Flexural Modulus | 18.1 GPa | 2630 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP VERTON RV00CEXS PA 66 LNP* VERTON* RV00CEXS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this grade include: Easy Molding, Structural. |