Polymer Property : Flexural Modulus = 176 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 176 GPa
25500 ksi
0°; ASTM D790
Zyvex Performance Materials Arovex™ 250 Carbon Nanotube Strengthened Prepreg
Arovex® 250 Prepreg is a 180°F (82°C) to 280°F (138°C) curing carbon nanotube strengthened epoxy prepreg suitable for numerous composites applications. Normal curing takes place at 250°F (121°..