Flexural Modulus 1.179 GPa
171.0 ksi
ASTM D790
Lucent Polymers TPO-30T Thermoplastic Polyolefin, 30% Mineral Filled
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.