Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 17.93 GPa | 2601 ksi | ASTM D-790 |
PlastiComp Complet® LCF20/LGF20 – PA66 BLK Polyamide 66, 40% Long Carbon/Glass Fiber Composite PelletsInformation provided by PlastiComp, Inc. |
|||
Flexural Modulus | 17.93 GPa | 2601 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 17.93 GPa | 2601 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI (Asia Pacific) LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |