Mechanical Properties Metric English Comments
Flexural Modulus 17.45 GPa

@Temperature 60.0 °C
2531 ksi

@Temperature 140 °F
ASTM D790
LATI LARTON G/50 50% Glass Fiber Filled Polyphenylene sulfide (PPS)  (discontinued **)
Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex..