Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 17.16 GPa | 2489 ksi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON RX04493D PA 66 LNP* VERTON* RX04493D is a compound based on Nylon 66 resin containing proprietary fillers. Added feature of this grade is: Structural. |
|||
Flexural Modulus | 17.16 GPa | 2489 ksi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON RX04493D PA 66 (Asia Pacific) LNP* Verton* RX04493D is a compound based on Nylon 66 resin. |