Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.12 GPa | 162 ksi | ASTM D790 |
Covestro Baydur® 726 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Flexural Modulus | 1.12 GPa | 162 ksi | ASTM D790 |
Braskem CP 144 Coating Polypropylene Information provided by Braskem |