Polymer Property : Flexural Modulus = 1617 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 11.15 GPa
1617 ksi
ISO 178
SABIC Innovative Plastics LNP Verton MX03017 PP (Europe-Africa-Middle East)
LNP* VERTON* MX03017 is a compound based on Polypropylene resin containing Glass Fiber, Long Glass Fiber. Added features of this material include: Chemically Coupled.This data was supplied by SABIC..