Polymer Property : Flexural Modulus = 16.45 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 16.45 GPa
2386 ksi
Plastcom SLOVAMID 6 GF 65 PA6, 65% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..