Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 16.05 GPa | 2328 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON OE004AE PPS - Branched LNP STAT-KON* OE004AE is a compound based on PPS - Branched resin containing 20% Carbon Fiber. Added features of this material are: Easy Molding, Electrically Conductive. |