Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 10.97 GPa
1591 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DF008ER PC
LNP THERMOCOMP* DF008ER is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features include: Easy Molding, Mold Release.
Flexural Modulus 10.97 GPa
1591 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DF008ERH PC
LNP THERMOCOMP* DF008ERH is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare.