Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 11.0 GPa | 1590 ksi | ASTM D790 |
Polymer Resources NY66-G43 Nylon 66, 43% Glass Reinforced Nylon 66, 43% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Flexural Modulus | 11.0 GPa | 1590 ksi | ASTM D790 |
Polymer Resources NY66-G43-[color]-H Nylon 66, 43% Glass Reinforced, Heat Stabilized Nylon 66, 43% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo.. |
|||
Flexural Modulus | 10.96 GPa | 1590 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP KONDUIT PX09322 PA 6 (Asia Pacific) White colored thermally conductive mineral filled PA6 FR compound |
|||
Flexural Modulus | 11.0 GPa | 1590 ksi | ASTM D790 |
Polymer Resources NY66-G43-[color]H Nylon, 43% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Modulus | 10.96 GPa | 1590 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP OX88533 PPS LNP LUBRICOMP* OX88533 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |