Polymer Property : Flexural Modulus = 157.8 ksi
Polymer Property :
Flexural Modulus =
157.8 ksi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
1.088
GPa
157.8
ksi
ASTM D790
Kolon KOCETAL® EL306 Toughened Grade Acetal Resin
Flexible grade. Applications: Flexible products. Information provided by API-Kolon.