Mechanical Properties Metric English Comments
Flexural Modulus 10.80 GPa
1567 ksi
CMT Materials METAPOR® HD 210 AL Air Permeable Material
METAPOR® is a composite material made of aluminum granules and epoxy resin. The material is air-permeable over the entire surface due to its micro-porous structure allowing for unique design consi..
Flexural Modulus 10.80 GPa
1567 ksi
ASTM D790
Omni Plastics OmniLon™ 6 PA6 GR15 WF25 Glass/Mineral Filled Nylon
Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics