Mechanical Properties Metric English Comments
Flexural Modulus 0.245 - 1.05 GPa
35.5 - 152 ksi
Average value: 0.676 GPa Grade Count:43
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade". Each property range of values report..