Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.021 GPa | 148.1 ksi | Method 1, Proc. B; ASTM D-790-95 |
Multibase Multi-Flex® TPO D 5305 Multi-Flex® D 5303 is a TOP compound for automotive applications such as bumper covers and side panels.Data provided by Multibase. |