Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.149 GPa | 1472.0 ksi | ISO 178 |
Ecomass® 4301ZC82 Stainless Steel Filled Polyphthalamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsStainless Steel Powder Filled Polyphthalamide (PPA)Very Good ToughnessInformation provided by Technical Po.. |