Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 12.8 - 13.6 GPa | 1860 - 1970 ksi | |
Bulk Molding Compounds BMC SLC 2000 Glass Reinforced Polyester BMC SLC 2000 is a medium strength, low-cost, glass reinforced polyester compound with adjustable shrinkage. Ideal for circuit breakers, motor switch housings, fuse holders, brush holders, standoff i.. |