Mechanical Properties Metric English Comments
Flexural Modulus 2.96 - 13.4 GPa
430 - 1950 ksi
Average value: 8.50 GPa Grade Count:13
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an..