Polymer Property : Flexural Modulus = 13.31 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 13.31 GPa
1930 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP VERTON RV00AE PA 66
LNP* VERTON* RV00AE is a compound based on Nylon 66 containing 50% Long Glass Fiber. Added features of this grade include: Easy Molding, Structural.