Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 12.61 GPa | 1829 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON AE004 ABS (Asia Pacific) LNP* STAT-KON* AE004 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |