Polymer Property : Flexural Modulus = 12.49 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 12.49 GPa
1812 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP QCL34 PA6.10
LNP* LUBRICOMP* QCL34 is a compound based on Nylon 6/10 resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive.