Mechanical Properties Metric English Comments
Flexural Modulus 12.38 GPa
1796 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP PF00A PA 6
LNP THERMOCOMP* PF00A is a compound based on Nylon 6 resin containing 50% Glass Fiber.
Flexural Modulus 12.38 GPa
1796 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP PF00A PA 6 (Asia Pacific)
LNP THERMOCOMP* PF00A is a compound based on Nylon 6 resin containing Glass Fiber.
Flexural Modulus 12.38 GPa
1796 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP PF00ASXS PA 6
LNP THERMOCOMP* PF00ASXS is a compound based on Nylon 6 resin containing 50% Glass Fiber. Added features of this material include: Heat Stabilized.
Flexural Modulus 12.38 GPa
1796 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP PF00ASXS PA 6 (Asia Pacific)
LNP THERMOCOMP* PF00ASXS is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.