Polymer Property : Flexural Modulus = 12.06 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 12.06 GPa
1749 ksi
ASTM D 790
SABIC Innovative Plastics Valox® VC120 PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 12.06 GPa
1749 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP UF0069S PPA
LNP THERMOCOMP* UF0069S is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized.