Polymer Property : Flexural Modulus = 1175 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 8.100 GPa
1175 ksi
Secant; ASTM D790
Fiberfil® FPI-33 BK Nylon 6, 33% Glass Reinforced, post industrial
Information provided by FIBERFIL Engineered Plastics
Flexural Modulus 8.100 GPa
1175 ksi
Secant; ASTM D790
Fiberfil® M-2271 NAT Nylon 6, 33% Glass Reinforced, post industrial, natural
Information provided by FIBERFIL Engineered Plastics