Polymer Property : Flexural Modulus = 1169 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 8.063 GPa
1169 ksi
ASTM D790
A. Schulman SCHULADUR® A GF33HI 33% Glass Fiber Reinforced, High Impact PBT
Information provided by A. Schulman.
Flexural Modulus 8.063 GPa
1169 ksi
ASTM D790
A. Schulman SCHULADUR® A GF33HI 33% Glass Fiber Reinforced, High Impact PBT
Information provided by A. Schulman.
Flexural Modulus 8.063 GPa
1169 ksi
ASTM D790
A. Schulman SCHULADUR® A GF33HI 33% Glass Fiber Reinforced, High Impact PBT
Information provided by A. Schulman.
Flexural Modulus 8.063 GPa
1169 ksi
ASTM D790
A. Schulman SCHULADUR® A GF33HI 33% Glass Fiber Reinforced, High Impact PBT
Information provided by A. Schulman.
Flexural Modulus 8.063 GPa
1169 ksi
ASTM D790
A. Schulman SCHULADUR® A GF33HI 33% Glass Fiber Reinforced, High Impact PBT
Information provided by A. Schulman.
Flexural Modulus 8.063 GPa
1169 ksi
ASTM D790
A. Schulman SCHULADUR® A GF33HI 33% Glass Fiber Reinforced, High Impact PBT
Information provided by A. Schulman.