Flexural Modulus 7.9461 GPa
1152.5 ksi
ASTM D790
E-Polymers SEPAZ® K115HF 15% Glass Fiber Reinforced High Flow PPS Resin
Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit..