Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 11.95 GPa | 1733 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF0069XZ PA 66 LNP THERMOCOMP* RF0069XZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant. |