Polymer Property : Flexural Modulus = 11.94 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 11.94 GPa
1732 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RFP38 PA6.6
LNP* LUBRICOMP* RFP38 is a compound based on Nylon 66 containing 40% Glass Fiber, 15% PTFE/Silicone. Added feature of this grade is: Wear Resistant.
Flexural Modulus 11.94 GPa
1732 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP ZF0089 PPE+PS
LNP* THERMOCOMP* ZF0089 is a compound based on PPE+PS resin containing 40% Glass Fiber. Added features of this material include: Exceptional Processing, Flame Retardant.