Flexural Modulus | 11.45 GPa | 1661 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP ZF406XXX PPO Blend LNP THERMOCOMP* ZF406XXX is a compound based on PPO Blend resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant. |
|||
Flexural Modulus | 11.45 GPa | 1661 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP ZF406XXX PPO Blend (Asia Pacific) LNP THERMOCOMP* ZF406XXX is a compound based on PPO Blend resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant. |